The differences in oxygen-free copper used in national-standard cables

Release time: 2026-06-11


Copper rod is the primary raw material in the cable industry, and it is produced mainly by two methods: continuous casting–rolling and upward continuous casting. Because these two processes differ, the oxygen content and surface appearance of the resulting copper rods vary. When properly executed, upward continuous casting can yield copper rods with an oxygen content below 10 ppm, which are referred to as oxygen-free copper rods.

Low-oxygen copper rod

I. Process Defects

Electrolytic copper is melted as it is added; the molten copper cannot undergo sufficient reduction, and throughout both the melting and tapping processes, oxygen must be excluded, resulting in a very high oxygen content. The fuel used for melting copper is typically gaseous; during combustion, such gases directly affect the chemical composition of the molten copper, with particularly significant impacts from sulfur and hydrogen.

II. Advantages of the Process

(1) High production capacity: typically, small-scale units can produce 10–14 tons per hour.

(2) The copper rod unwinding adopts a plum-blossom pattern, facilitating wire feeding by the wire-drawing machine.

(3) The coiled wire has a substantial weight, typically reaching up to 4 tons per coil.

III. Grades and Properties of Low-Oxygen Copper Rods

There are three grades of low-oxygen copper rod: T1, T2, and T3. All low-oxygen copper rods are hot-rolled, making them soft rods, designated by the code “R.”

(1) T1: Low-oxygen copper rods are produced using high-purity electrolytic copper as the raw material (with a copper content exceeding 99.9975%).

(2) T2: Low-oxygen copper rods are produced using #1 electrolytic copper as the raw material (with a copper content exceeding 99.95%).

(3) T3: Low-oxygen copper rods are produced using #2 electrolytic copper as the raw material (with a copper content exceeding 99.90%). Since high-purity electrolytic copper and #2 electrolytic copper are scarce on the market, #1 electrolytic copper is typically used instead; consequently, the standard grade for low-oxygen copper rods is generally designated as T2R.

Oxygen-free copper rod

I. Introduction

Oxygen-free copper rod is pure copper that contains neither oxygen nor any residual deoxidizers. In practice, however, it still contains trace amounts of oxygen and certain impurities. According to the standard, the oxygen content shall not exceed 0.02%, the total impurity content shall not exceed 0.05%, and the copper purity shall be greater than 99.95%.

It is typically produced from electrolytic copper and has a lower resistivity than low-oxygen copper rod; therefore, in the manufacture of products with stringent electrical resistance requirements, oxygen-free copper rod is more cost-effective. Producing oxygen-free copper rod, however, necessitates higher‑grade raw materials.

Based on oxygen and impurity levels, oxygen-free copper rods are further classified into TU1 and TU2 grades. TU1 oxygen-free copper rods achieve a purity of 99.99%, with an oxygen content not exceeding 0.001%; TU2 oxygen-free copper attains a purity of 99.95%, with an oxygen content no greater than 0.002%.

II. Differences Between the Two

Due to differences in their manufacturing processes, low-oxygen copper rods and oxygen-free copper rods exhibit distinct properties and each has its own unique characteristics.

(1) Oxygen inhalation, removal, and its state of existence

The oxygen content of low‑oxygen copper rods typically ranges from 200 (175) to 400 (450) ppm; thus, oxygen is absorbed during the liquid phase of copper. In contrast, oxygen‑free copper rods produced by the upward‑drawing process have their oxygen reduced and removed after it has remained in the liquid state for a considerable period. Such rods generally exhibit an oxygen content below 10–50 ppm, with the lowest levels reaching as low as 1–2 ppm. Due to its extremely low oxygen content, oxygen‑free copper possesses a uniform, single‑phase microstructure that is favorable for toughness.

(2) The difference between the amount of foreign matter and the existing hot-rolling defects.

The drawability of oxygen‑free copper rods is superior to that of low‑oxygen copper rods across all wire diameters. In addition to the microstructural factors mentioned above, oxygen‑free copper rods contain fewer inclusions, exhibit stable oxygen levels, and are free from defects that can arise during hot rolling. By contrast, inadequate oxygen monitoring and fluctuating oxygen content can directly compromise rod performance. While surface oxides on the rod may be removed through continuous cleaning in subsequent processes, a more troublesome issue is the presence of substantial oxide layers beneath the surface, which have a more direct adverse impact on wire‑drawing breakage.

(3) There is a difference in toughness between low-oxygen copper rods and oxygen-free copper rods.

Both can be drawn to 0.015 mm, but in low‑temperature superconducting wires, the low‑grade oxygen‑free copper has a strand spacing of only 0.001 mm.

(4) The wire-drawing processes for low-oxygen and oxygen-free copper rods differ.

The wire-drawing process for low‑oxygen copper rods cannot be directly applied to that of oxygen‑free copper rods; at the very least, their annealing processes differ. Since wire softness is strongly influenced by material composition as well as the rod‑making, wire‑drawing, and annealing procedures, it is not appropriate to simply conclude that low‑oxygen copper is softer or harder than oxygen‑free copper.